Heat Transfer Printing Hot Melt Powder For Screen Printing

Heat Transfer Printing Hot Melt Powder For Screen Printing

  • Color
    White
  • Composition
    Polyurethane
  • Appearance
    Powder
  • Melt Point(DSC)
    105-115℃
  • Melt Flow Index
    30±7g/10min
  • Washable Property
    60 ℃
  • Powder Size Range
    0-80 μm; 80-300 μm;100-400 μm
  • Density
    1.21±0.02 G/cm3
  • Hardness
    83±3 Shore A
  • Packaging
    25KG In One PE Bag+Brown Paper
  • Product Type
    TPU Hot Melt Adhesive Powder
  • Place of Origin
    China
  • Brand Name
    Easun
  • Certification
    Rosh, Reach
  • Model Number
    ES226
  • Minimum Order Quantity
    25KG
  • Price
    Negotiable
  • Packaging Details
    20KG/bag
  • Delivery Time
    3-8 working day
  • Payment Terms
    T/T
  • Supply Ability
    4000000

Heat Transfer Printing Hot Melt Powder For Screen Printing

Heat Transfer Printing Hot Melt Powder For Screen Printing

 

Product model: ES226

 

Description:This product is a copolyester thermoplastic powdery hot melt adhesive. Soft hand feel and certain resilience, excellent processability. Excellent adhesion to textiles, PVC, PC.

 

Function:Heat transfer,Digital printing,Silk screen printing.

 

TPU Hot Melt Adhesive Powder Physical Characteristics:

 

Property Criterion
Appearance White powder
Composition TPU
Density ASTM D-792 1.2±0.02g/cm³
Melt Point DSC 105-115 ℃
Melt Index ASTM D-1238 30±5g/10min
Powder size range 0-80 um
0-170 um
80-200 um
125-200 um
150-250 um
180-420 um

 

Technical Parameters:

 

Bonding parameters (for reference only) Temperature 105-120℃
Press 3.0 kg/cm2
Time 14S
Washing Resistance 40℃ Excellent
60℃ good
90℃ /

 

TPU Hot Melt Adhesive Powder Packaging and Storage Conditions:

Packaging 25KG in one PE bag+Brown paper bag
Storage Conditions Stored in dry unopened packaging at room temperature for 12 months. High temperature and pressure will cause agglomeration. The trays cannot be double-pressed.


1. Bonding temperature and pressure and time relate to the bonding strength of the film to the material. The bonding temperature must be close to the temperature set by the machine, the pressure must be uniform, and the mold and press rolls must be flat.

2. The bonding conditions used will vary between machines and materials. The conditions indicated here are only basic. The most ideal bonding conditions should be established by manufacturing for the specific application.

 